DIFFERENTIAL THERMAL
ANALYSIS
&
DIFFERENTIAL SCANNING
CALORIMETRY
Smt. Kishoritai Bhoyar College of Pharmacy, Kamptee
INTRODUCTION
Differential thermal analysis is a technique
measuring the difference in temperature between a
sample and reference (a thermally inert material) as a
function of the time or the temperature, when they
undergo temperature scanning in a controlled
atmosphere. The DTA method enables any
transformation to be detected for all the categories of
materials.
Here,
Differential temperature ∆T (Temperature difference between
sample temperature Ts & reference temperature Tr.)
∆T = Ts – Tr
Reference temperature Tr or furnace temperature Tf & ∆T is
plotted as a function of time.
DTA
curve
From the graph,
▪ Sharp exothermic peaks give the ideas of changes in
crystallity or fusion process.
▪ Chemical reaction (Oxidative reaction) shows Exothermic
curve.
▪ Broad endothermic peaks gives signifying dehydration
reaction.
▪ Physical changes shows Endothermic curve.
▪ DTA curve would be parallel to the temperature (or time)
axis till the sample undergo any physical or chemical
changes.
INSTRUMENTATION
Component of a DTA apparatus
 Furnace
 Sample Holder
 DC Amplifier
 Differential Temperature Detector
 Furnace Temperature Programmer
 Recorder
 Control Equipment
Diagram of DTA apparatus
SAMPLE HOLDER
1.Material
Criteria for selection of material
▪ Cost
▪ Ease of fabrication
▪ Inertness towards the reactants & product in the
temperature range.
Types of material
➢ Metallic material:
High thermal conductivity
Ex. Nickel, Stainless steel (up to 1000oC),
Platinum and its alloys.
Give sharp exotherm and flat endotherm.
➢ Non metallic material:
Low thermal conductivity
Ex. Glass,Vitrous silica or sintered alumina.
Give flat exotherm and sharp endotherm.
Generally platinum is used.
Disadvantage: Catalyses many reactions.
2. Geometry
Ideal geometry around thermocouple junction is
spherical but show problem in fabricaion.Hence
cylindrical shape generally used.
 Types of sample holders
Sample holder with dimples
in which thermocouple
junctions are inserted,dimples
known as thermocouple well.
To investigate several
samples simultaneously
blocks with symmetrically
located multiple
compartments have been
designed.
The reference
temperature may be
measured either at the
center of reference or
sample using
respective arm of the
differential
thermocouple in (A)
By a separate
thermocouple in block
(B)
(A)
(B)
 Polyp late sample holder and wire gauge
crucibles are used for a good exchange of gases
with the enveloping environment, where the solid
gas reactions are influenced by the partial pressure
of the gaseous reactant or product.
FURNACE
The choice of furnace geometry and heating
element mainly depend upon the length of uniform
temperature zone desired.
The furnace which cover the range
from -1900C to 28000C
Heated by
A resistance element: nichrome, platinum ,rhodium
globar, molybdenum and tungsten.
IR Radiation
High frequency RF oscillator
By a coil of tubing through which a heated or
cooled liquid or gas is circulated.
Always prefer tubular furnace.
 A relation between the power demand P in watts, furnace
dimension and temperature for a cylindrical tubular
furnace.
P = 2.729Km (T1 – T2) l
log d2 / d1
Where, l = length in cm
Km= Average thermal conductivity coefficient of
the insulation(Watt/cm2. K)
d1=Diameter of the heater coil wound on the
ceramic
d2=Diameter of furnace shell
T1&T2=Temperature of heating element and
surface temperature of the furnace shell
TEMPERATURE CONTROLLER & RECORDER
Temperature control
To control temperature, three basic elements
are required.
➢ Sensor
➢ Control element
➢ Heater
Control element governs the rate of heat input
match with heat loss from the system.
Two methods for controlling temperature:
On-Off control: In this device, if the sensor
signal indicates that the temperature increases
than the set point, then the heater immediately
cut off.
Not use in DTA(Reason-Electrical interference
affect measurement of signals).
Proportional control: The heat input to the
system is progressively reduced as the
temperature approaches to the desired value.
such controller that anticipates to set value is
known as “proportional controller”
Temperature Programmer
To produce desired rate of heating, cooling and to
maintain the constant temperature at any desired value,
thermal apparatus require time dependent temperature
cycling of the furnace.
To achieve this, a temperature programmer which
transmits a certain time based instruction to control unit.
Recorder
The signals obtained from the sensor recorded. Signal
trace is produce on paper or film ,heating stylus,
electrical writing or optical beam.
▪ Deflection type
▪ Null type
I) Deflection Balances:-
a) Beam type:- In this type of
balance, the conversion of
beam deflection about the
fulcrum into suitably
identified weight change
curve by photographic
recorded trace.
b) Helical or spring balance:- In
this type, the elongation or
contraction of spring with
weight change can be
determined.
c)Cantilever type:- In this one
of the beam is fixed & other
end on which sample is to
be placed is free to undergo
deflection.
d)Torsion type:- Beam is
attached to the taut wire
which act as fulcrum. The
wire is finally fixed at both
the end so that the
deflection of beam are
proportional to weight
change & tortional strain
of wire.
II)Null Point Balance:-
▪ In this type there is sensor to detect deviation of the balance
beam from the null position.
▪ The restoring force either electrical or mechanical weight
loading is applied to restore its null position from the
horizontal norm.
▪ The force is directly proportional to weight change.
THERMOCOUPLE (TEMPERATURE SENSOR)
Selection criteria :
 Temperature interval
 Thermoelectric coefficient
 Chemical capability with sample
 Chemical gaseous environment used and
reproducibility of EMF Vs. Temperature curve
as a function of thermal cycling.
 Availability and cost
THERMOCOUPLE TEMPERATURE
Copper couple Up to 3000C
Cromel - alumel
couple
Up to 10000C
Platinum couple Up to 15000C
Tungsten & Rhenium
in inert gas
or vacuum
Up to 21000C
(not for general use)
FACTORS AFFECTING ON DTA CURVE:
Environmental :-
The DTA technique is more sensitive to gases around sample than TG.
Reaction of gases with sample may give extra peaks in curve (i.e.
oxygen in air gives oxidation reaction producing exothermic peaks).
So to control such reaction DTA studies used two type of gaseous
atmosphere.
▪Static
▪Dynamic
▪ Static:-it is difficult to reproduce because atmosphere surrounding the
sample changing in the concentration chemically due to evolved gases
and physically due to convention current therefore the studies in the
static gaseous environment is imprecise.
▪ Dynamic:- Easy to reproduced. gases are swept pass the sample at
controlled way are reliable and reproducible. This swept gases are
either inert or reactive.
Instrumental:-
a)Sample holder:- Geometry & the material used in the fabrication of
the sample affects the resolution , shape, size of the DTA peaks.
❑ If sample holder made up of ,
1. High thermal conductivity material (metal)- sharp exothermic but
relatively flat endothermic peak .
2. Poor thermal conductivity material (ceramic)-the reveres will
happen.
For better resolution the size of the holder and amount of sample
should be as small as possible.
b)Differential temperature sensing devices:- Generally wires are
used.
1. If thick wire is used:- more distortion of peak height & peak
temperature.
2. If thinner:- lesser distortion in peak height and peak temperature.
c) Furnace characteristics:-
1. Type of winding directly affects the DTA curve. If the
winding used in furnace is not uniform, the base line
is changed. This type of effect is generally seen in
hand wound furnaces.
i) Grooved muffled cores furnace is used because it
insure uniform winding.
ii) Biflar winding also used because it minimize the
magnetic pick-up encountered with on –off controller.
d) Temperature programmer controller:-
Switching on –off type controller are not used because
it produces noise at a particular temperature range
i.e. a. bow 700oc.
Motor driver is used.
e) Thermal Regime:-
➢ Heating rate influence the DTA curve.
➢ Higher the heating rates ,higher the peak temperature&
sharper the peak intensity.
Generally heating rate of 100 to 200 per minute are employed.
f) Recorder:-
➢ Type, span, chart-speed and pen response ,sensitivity of
recorder affect the DTA curve.
➢ Span is not proper then necessary to preamplify the signals.
➢ If sensitivity is not properly selected, weaker signals would
not be recorded whereas stronger signals might be
damping.
➢ If faster chart-speeds used , DTA curve gets flattened.
 Sample characteristics:-
a) physical:-
▪ one assumption that heat capacity remain constant with the
progress of reaction but it changes with progress of reaction.
▪ To maintain the heat capacity nearly constant , the usual
sample is mixed with an excess amount of an inert material.
But it create some problems.
▪ Partial size affects the peak area , it deceases with increasing
particle size.
▪ Partial size affects the peak temperature. Increase particle size
the peak temperature is shifted to higher value.
▪ Weight of sample also affect the peak intensity &
temperature. Both this increases with increasing
weight.
▪ To minimize all this problems sample is mixed with
a diluents.
b) Chemical :-
➢ The chemical reactivity of sample, sample holder,
thermocouple material, the ambient gaseous environment and
added diluents alters the DTA curve(peaks) .
➢ Select this material inert chemically as possible.
APPLICATION
1. Physical chemistry
a. Heat of Reaction:
Borchardt & Daniels concluded that the peak area A in
DTA is always a linear function of the heat of reaction,
∆H, when the rate of heat of production or consumption is
a function only of time.
The heat of reaction per mole is given by
∆H =KA/N0
Where, N0 = Initial no. of moles
K= Constant (Calibration coefficient)
b. Specific heat
DTA used to determine the specific heat of substance like
naphthalene.
The Cp was determined by following formula:
KK| (b – a)
Cp =
d ms dt
where,
K & K| = Constant (determined from
calibration curve of standard substance)
d = Density of sample
ms = Mass of sample
dt = The temperature interval over which
Cp is measured.
c. Thermal diffusivity
To determine thermal diffusivities by measuring
the temperature difference ,∆T,
between the center and surface of the sample, heated
at uniform rate.
The difference in temperature was measured by
using differential thermocouple.
ß r2
D =
6 ∆Ts
where,
r = Radius of spherical sample cavity
ß = Heating state
2. Analytical Chemistry
a. Polymer analysis
Analysis of a polymer shows several features due to physical and
chemical changes, including:
 Glass transition: Transition from disordered solid to liquid,
glassy, amorphous polymer becomes flexible, H = 0, but change in Cp.
 Crystallization of amorphous polymer into microcrystal is
exothermic. Disordered to ordered transition.
 Melting of polymer crystal. Ordered to disordered transition
Oxidation peak would be absent in N2 atmosphere

T
b. To fingerprint substances
DTA of (a) butter and (b) margarine
temp →
a
b
c. To determine M.Pt., B.Pt., decomposition temperatures of
organic compounds
DTA of benzoic acid
A ambient pressure;
B 200 lb in-2 pressure
3. Quality control
DTA technique used for quality control of substance like
cement, glass, oil, catalysts, textile, explosives, resins ,
etc.
 Characterization of limestone used in Portland cement
 To control amount of magnesium carbonate in cement
 To establish slag content present in a mixture of
Portland cement & blast furnace slag
 Characterization of gypsum plasters & corcidolite.
4.INORGANIC CHEMISTRY
 To study the thermal stability of large number of
inorganic compound and complexes.
 To study oxalates, metal amine complexes,
carbonates and oxides.
 To study the oxides of uranium and plutonium.
Uranium dioxide powder with good sintering
qualities has been observed to give well defined
and well separated DTA peaks.
 Advantages:
• instruments can be used at very high
temperatures
• instruments are highly sensitive
• flexibility in crucible volume/form
• characteristic transition or reaction
temperatures can be accurately determined
 Disadvantages:
• uncertainty of heats of fusion, transition, or
reaction estimations is 20-50%
• less satisfactory than DSC with regard to
resolution of thermal traces and qualitative
data.
INTRODUCTION
Differential scanning calorimetric is a technique
determining the variation in the heat flow given out
or taken in by a sample as a function of temperature
or time.
The DSC curve is recorded with the chart
abscissa indicating the transition temperature . The
area of peak measures the total energy transfer to or
from the sample.
INSTRUMENTATION
➢ A typical DSC consists of two sealed pans: a sample
pan and a reference pan(empty). These pans are often
covered by or composed of aluminum, which acts as a
radiation shield. The two pans are heated, or cooled,
uniformly while the heat flow difference between the
two is monitored.
➢ This can be done at a constant temperature
(isothermally), but is more commonly done by
changing the temperature at a constant rate, a mode of
operation also called temperature scanning.
➢ The instrument detects differences in the heat flow
between the sample and reference.
➢ This information is sent to an output device, most
often a computer, resulting in a plot of the differential
heat flow between the reference and sample cell as a
function of temperature. the differential heat flow is
calculated by subtracting the sample heat flow from
the reference heat flow.
➢ The sample is generally placed in an aluminum sample
pan. The reference consists of a matched empty
aluminum sample pan that is placed in the reference
cell of the instrument. The sample pans are designed to
have a very high thermal conductivity.
➢ Sample sizes generally range from 0.1 to 100 mg. This
also allows experiments to be performed under
variable pressures and atmospheres.
TYPES OF DSC INSTRUMENT
1.Heat Flux DSC:-
sample
pan
inert gas
vacuum
heating
coil
reference
pan
thermocouples
chromel wafer
constantan
chromel/calomel
wires
crimped Al pans (<500 o C)
▪ sample holder : sample and reference are connected by
a low-resistance heat flow path
Al or Pt pans placed on constantan disc
▪ Sensors: Chromel®-constantan area thermocouples
(differential heat flow)
Chromel®-alumel thermocouples (sample temperature)
▪ Furnace: One block for both sample and reference cells
▪ temperature controller: temperature difference between the
sample and reference is converted to differential thermal
power, did/dot, which is supplied to the heaters to maintain
the temperature of the sample and reference at the program
value
2.Power Compensated DSC
sample
pan
T = 0
inert gas
vacuum
inert gas
vacuum
individual
heaters
controller P
reference
pan
thermocouple
 Sample holder:
Al or Pt pans
 Sensors:
Pt resistance thermocouples separate sensors
and heaters for the sample and reference
 Furnace:
separate blocks for sample and reference
cells
 Temperature controller:
differential thermal power is supplied to the
heaters to maintain the temperature of the
sample and reference at the program value
FACTORS AFFECTING DSC CURVES
a. Sample shape:
The shape of sample has little effect on quantitative
aspect but more effect on quality aspect.
Sample in the form of a disc film or powder spread
on the pan are preferred.
b. Sample size
0.5 to 10mg usually sufficient.
Smaller sample:
▪ Faster scanning
▪ Better shaped peak with good resolution
▪ Provide greater contact with the gaseous environment
Larger sample
 Smaller heat of transitions may be measured with greater
precision.
c. Power supply
;
Variation of power supply to
sample & reference
DSC curve
APPLICATION
DSC can be used for all application of conventional DTA.
Use in industry for small size of sample
To detect phase changes and decompositions.
Ex.- DTA & DSC of CuSO4 .5H2O
DTA DSC
To study the oxidative stability of samples generally
requires an airtight sample chamber. Usually, such tests are
done isothermally (at constant temperature) by changing
the atmosphere of the sample. First, the sample is brought
to the desired test temperature under an inert atmosphere,
usually nitrogen. Then, oxygen is added to the system. Any
oxidation that occurs is observed as a deviation in the
baseline. Such analyses can be used to determine the
stability and optimum storage conditions for a compound.
Consequently, less pure compounds will exhibit a
broadened melting peak that begin sat lower temperature
than a pure compound.
In the pharmaceutical industry it is necessary to
have well-characterized drug compounds in order to
define processing parameters. For instance, if it is
necessary to deliver a drug in the amorphous form, it is
desirable to process the drug at temperatures below
those at which crystallization can occur.
In food science research, DSC is used in conjunction
with other thermal analytical techniques to determine
water dynamics. Changes in water distribution may
be correlated with changes in texture. Similar to
material science studies, the effects of curing on
confectionery products can also be analyzed.
In last few years this technology has been involved
in metallic material study. It is known that it is
possible to use DSC to find solids and liquids
temperature of a metal alloy, but the widest
application is, by now, the study of precipitations,
Gainer Preston zones, phase transitions,
dislocations movement, grain growth etc.
For the polymer chemist, DSC is a handy tool for
studying curing processes, which allows the fine
tuning of polymer properties. The cross-linking of
polymer molecules that occurs in the curing process
is exothermic, resulting in a positive peak in the DSC
curve that usually appears soon after the glass
transition.
DSC curves may also be used to evaluate drug and
polymer purities. This is possible because the
temperature range over which a mixture of compounds
melts is dependent on their relative amounts. This effect
is due to a phenomenon known as freezing point
depression, which occurs when a foreign solute is added
to a solution.
Used in the study of liquid crystals. As matter transitions
between solid and liquid it often goes through a third state,
which displays properties of both phases. This anisotropic
liquid is known as a liquid crystalline or mesomorphous
state. Using DSC, it is possible to observe the small energy
changes that occur as matter transitions from a solid to a
liquid crystal and from a liquid crystal to an isotropic liquid.
 Advantages
• Smaller sample required.
• Good qualitative data on phase changes.
 Disadvantages
• Limited to small sample size
• Thermograms are often complex and thus
difficult to interpret fully
COMPARISON OF DTA AND DSC
Aspect DSC DTA
Size of sample 2 to 10mg 20 to 50 mg
Sensitivity of
measurement of
heat of transition
A few joules/mole 0.5 Kj/mole
Heating and cooling
cycle
Programmed
heating and cooling
possible
Generally
programmed
heating.
Second order phase
transition
It can be observed
with a sample size
of 200mg
Not observed.
Specific heat
measurement
Accurate Not accurate
Differential Thermal Analysis & Differential Scanning Calorimetry

Weitere ähnliche Inhalte

Was ist angesagt?

Presentation2dsc
Presentation2dscPresentation2dsc
Presentation2dsc
Srota Dawn
 

Was ist angesagt? (20)

DSC & TGA Thermal Analysis.pptx
 DSC & TGA  Thermal Analysis.pptx DSC & TGA  Thermal Analysis.pptx
DSC & TGA Thermal Analysis.pptx
 
DIFFERENTIAL THERMAL ANALYSIS (DTA), ppt
DIFFERENTIAL THERMAL ANALYSIS (DTA),  pptDIFFERENTIAL THERMAL ANALYSIS (DTA),  ppt
DIFFERENTIAL THERMAL ANALYSIS (DTA), ppt
 
Differential Scanning Colorimetry
Differential Scanning ColorimetryDifferential Scanning Colorimetry
Differential Scanning Colorimetry
 
DSC and DTA
DSC and DTADSC and DTA
DSC and DTA
 
Thermogravimetric analysis ppt
Thermogravimetric analysis pptThermogravimetric analysis ppt
Thermogravimetric analysis ppt
 
Differential Thermal Analysis (DTA)
Differential Thermal Analysis (DTA)Differential Thermal Analysis (DTA)
Differential Thermal Analysis (DTA)
 
Differential Scanning Calorimetry (DSC)
Differential Scanning Calorimetry (DSC)Differential Scanning Calorimetry (DSC)
Differential Scanning Calorimetry (DSC)
 
Differential scanning calorimetry [dsc]
Differential scanning calorimetry [dsc]Differential scanning calorimetry [dsc]
Differential scanning calorimetry [dsc]
 
Differential scanning calorimetry
Differential scanning calorimetryDifferential scanning calorimetry
Differential scanning calorimetry
 
Instrumentation of Thermogravimetric Analysis
Instrumentation  of  Thermogravimetric Analysis Instrumentation  of  Thermogravimetric Analysis
Instrumentation of Thermogravimetric Analysis
 
Presentation2dsc
Presentation2dscPresentation2dsc
Presentation2dsc
 
thermogaravimetric analysis differential thermal analysis swapnil ppt
thermogaravimetric analysis differential thermal analysis swapnil pptthermogaravimetric analysis differential thermal analysis swapnil ppt
thermogaravimetric analysis differential thermal analysis swapnil ppt
 
Differential Thermal Analysis (DTA)
Differential Thermal Analysis (DTA)Differential Thermal Analysis (DTA)
Differential Thermal Analysis (DTA)
 
DIFFERENTIAL THERMAL ANALYSIS (DTA)
DIFFERENTIAL THERMAL ANALYSIS (DTA)DIFFERENTIAL THERMAL ANALYSIS (DTA)
DIFFERENTIAL THERMAL ANALYSIS (DTA)
 
Diffrential scanning calorimery (dsc) ppt
Diffrential scanning calorimery (dsc) pptDiffrential scanning calorimery (dsc) ppt
Diffrential scanning calorimery (dsc) ppt
 
Differential Scanning Calorimeter Instrumentation.(DSC)
Differential Scanning Calorimeter Instrumentation.(DSC)Differential Scanning Calorimeter Instrumentation.(DSC)
Differential Scanning Calorimeter Instrumentation.(DSC)
 
Thermo gravimetric analysis(tga)
Thermo gravimetric analysis(tga)Thermo gravimetric analysis(tga)
Thermo gravimetric analysis(tga)
 
interpretation of NMR spectroscopy
interpretation of  NMR spectroscopyinterpretation of  NMR spectroscopy
interpretation of NMR spectroscopy
 
Thermogravimetric analysis
Thermogravimetric analysisThermogravimetric analysis
Thermogravimetric analysis
 
instrumentation of mass spectrometry
instrumentation of mass spectrometryinstrumentation of mass spectrometry
instrumentation of mass spectrometry
 

Ähnlich wie Differential Thermal Analysis & Differential Scanning Calorimetry

Differential Scanning Calorimetry (DSC).pdf
Differential Scanning Calorimetry (DSC).pdfDifferential Scanning Calorimetry (DSC).pdf
Differential Scanning Calorimetry (DSC).pdf
SanDeepSharma926061
 
Thermo analytical methods by srk
Thermo analytical methods by srkThermo analytical methods by srk
Thermo analytical methods by srk
Vaishnavi Patil
 

Ähnlich wie Differential Thermal Analysis & Differential Scanning Calorimetry (20)

thermogravimetric analysis
thermogravimetric analysisthermogravimetric analysis
thermogravimetric analysis
 
Tga
TgaTga
Tga
 
Thermal methods of Analysis
Thermal methods of  Analysis Thermal methods of  Analysis
Thermal methods of Analysis
 
A presentation on Thermal gravimetry analysis (TGA)
A presentation on Thermal gravimetry analysis (TGA)A presentation on Thermal gravimetry analysis (TGA)
A presentation on Thermal gravimetry analysis (TGA)
 
Thermal analysis 4
Thermal analysis  4Thermal analysis  4
Thermal analysis 4
 
TGA.pptx principle, instrumentation, theory
TGA.pptx principle, instrumentation, theoryTGA.pptx principle, instrumentation, theory
TGA.pptx principle, instrumentation, theory
 
Thermal analysis
Thermal analysis Thermal analysis
Thermal analysis
 
Tga
TgaTga
Tga
 
DTA
DTADTA
DTA
 
Thermo gravimetric analysis
Thermo gravimetric analysisThermo gravimetric analysis
Thermo gravimetric analysis
 
TGA TECHNIQUES.pptxhhhjjkkkhhhbbbbbbbnjjjn
TGA TECHNIQUES.pptxhhhjjkkkhhhbbbbbbbnjjjnTGA TECHNIQUES.pptxhhhjjkkkhhhbbbbbbbnjjjn
TGA TECHNIQUES.pptxhhhjjkkkhhhbbbbbbbnjjjn
 
Dta
DtaDta
Dta
 
Thermal analysis.pptx
Thermal analysis.pptxThermal analysis.pptx
Thermal analysis.pptx
 
TEMPERATURE MEASUREMENTS.pptx .
TEMPERATURE MEASUREMENTS.pptx              .TEMPERATURE MEASUREMENTS.pptx              .
TEMPERATURE MEASUREMENTS.pptx .
 
Differential thermal analysis - instrumental methods of analysis
Differential thermal analysis - instrumental methods of analysis Differential thermal analysis - instrumental methods of analysis
Differential thermal analysis - instrumental methods of analysis
 
Differential Scanning Calorimetry (DSC).pdf
Differential Scanning Calorimetry (DSC).pdfDifferential Scanning Calorimetry (DSC).pdf
Differential Scanning Calorimetry (DSC).pdf
 
Instrumentation
InstrumentationInstrumentation
Instrumentation
 
DTA AND DDTA AS PER PHARMA
DTA AND DDTA AS PER PHARMADTA AND DDTA AS PER PHARMA
DTA AND DDTA AS PER PHARMA
 
Thermo analytical methods by srk
Thermo analytical methods by srkThermo analytical methods by srk
Thermo analytical methods by srk
 
Thermo gravimetric Analysis
Thermo gravimetric AnalysisThermo gravimetric Analysis
Thermo gravimetric Analysis
 

Kürzlich hochgeladen

Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
ZurliaSoop
 

Kürzlich hochgeladen (20)

ICT Role in 21st Century Education & its Challenges.pptx
ICT Role in 21st Century Education & its Challenges.pptxICT Role in 21st Century Education & its Challenges.pptx
ICT Role in 21st Century Education & its Challenges.pptx
 
Beyond_Borders_Understanding_Anime_and_Manga_Fandom_A_Comprehensive_Audience_...
Beyond_Borders_Understanding_Anime_and_Manga_Fandom_A_Comprehensive_Audience_...Beyond_Borders_Understanding_Anime_and_Manga_Fandom_A_Comprehensive_Audience_...
Beyond_Borders_Understanding_Anime_and_Manga_Fandom_A_Comprehensive_Audience_...
 
Python Notes for mca i year students osmania university.docx
Python Notes for mca i year students osmania university.docxPython Notes for mca i year students osmania university.docx
Python Notes for mca i year students osmania university.docx
 
COMMUNICATING NEGATIVE NEWS - APPROACHES .pptx
COMMUNICATING NEGATIVE NEWS - APPROACHES .pptxCOMMUNICATING NEGATIVE NEWS - APPROACHES .pptx
COMMUNICATING NEGATIVE NEWS - APPROACHES .pptx
 
Sociology 101 Demonstration of Learning Exhibit
Sociology 101 Demonstration of Learning ExhibitSociology 101 Demonstration of Learning Exhibit
Sociology 101 Demonstration of Learning Exhibit
 
Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
Jual Obat Aborsi Hongkong ( Asli No.1 ) 085657271886 Obat Penggugur Kandungan...
 
Mehran University Newsletter Vol-X, Issue-I, 2024
Mehran University Newsletter Vol-X, Issue-I, 2024Mehran University Newsletter Vol-X, Issue-I, 2024
Mehran University Newsletter Vol-X, Issue-I, 2024
 
FSB Advising Checklist - Orientation 2024
FSB Advising Checklist - Orientation 2024FSB Advising Checklist - Orientation 2024
FSB Advising Checklist - Orientation 2024
 
Unit 3 Emotional Intelligence and Spiritual Intelligence.pdf
Unit 3 Emotional Intelligence and Spiritual Intelligence.pdfUnit 3 Emotional Intelligence and Spiritual Intelligence.pdf
Unit 3 Emotional Intelligence and Spiritual Intelligence.pdf
 
Single or Multiple melodic lines structure
Single or Multiple melodic lines structureSingle or Multiple melodic lines structure
Single or Multiple melodic lines structure
 
Basic Civil Engineering first year Notes- Chapter 4 Building.pptx
Basic Civil Engineering first year Notes- Chapter 4 Building.pptxBasic Civil Engineering first year Notes- Chapter 4 Building.pptx
Basic Civil Engineering first year Notes- Chapter 4 Building.pptx
 
Plant propagation: Sexual and Asexual propapagation.pptx
Plant propagation: Sexual and Asexual propapagation.pptxPlant propagation: Sexual and Asexual propapagation.pptx
Plant propagation: Sexual and Asexual propapagation.pptx
 
Graduate Outcomes Presentation Slides - English
Graduate Outcomes Presentation Slides - EnglishGraduate Outcomes Presentation Slides - English
Graduate Outcomes Presentation Slides - English
 
Food safety_Challenges food safety laboratories_.pdf
Food safety_Challenges food safety laboratories_.pdfFood safety_Challenges food safety laboratories_.pdf
Food safety_Challenges food safety laboratories_.pdf
 
This PowerPoint helps students to consider the concept of infinity.
This PowerPoint helps students to consider the concept of infinity.This PowerPoint helps students to consider the concept of infinity.
This PowerPoint helps students to consider the concept of infinity.
 
ICT role in 21st century education and it's challenges.
ICT role in 21st century education and it's challenges.ICT role in 21st century education and it's challenges.
ICT role in 21st century education and it's challenges.
 
Kodo Millet PPT made by Ghanshyam bairwa college of Agriculture kumher bhara...
Kodo Millet  PPT made by Ghanshyam bairwa college of Agriculture kumher bhara...Kodo Millet  PPT made by Ghanshyam bairwa college of Agriculture kumher bhara...
Kodo Millet PPT made by Ghanshyam bairwa college of Agriculture kumher bhara...
 
HMCS Max Bernays Pre-Deployment Brief (May 2024).pptx
HMCS Max Bernays Pre-Deployment Brief (May 2024).pptxHMCS Max Bernays Pre-Deployment Brief (May 2024).pptx
HMCS Max Bernays Pre-Deployment Brief (May 2024).pptx
 
TỔNG ÔN TẬP THI VÀO LỚP 10 MÔN TIẾNG ANH NĂM HỌC 2023 - 2024 CÓ ĐÁP ÁN (NGỮ Â...
TỔNG ÔN TẬP THI VÀO LỚP 10 MÔN TIẾNG ANH NĂM HỌC 2023 - 2024 CÓ ĐÁP ÁN (NGỮ Â...TỔNG ÔN TẬP THI VÀO LỚP 10 MÔN TIẾNG ANH NĂM HỌC 2023 - 2024 CÓ ĐÁP ÁN (NGỮ Â...
TỔNG ÔN TẬP THI VÀO LỚP 10 MÔN TIẾNG ANH NĂM HỌC 2023 - 2024 CÓ ĐÁP ÁN (NGỮ Â...
 
Application orientated numerical on hev.ppt
Application orientated numerical on hev.pptApplication orientated numerical on hev.ppt
Application orientated numerical on hev.ppt
 

Differential Thermal Analysis & Differential Scanning Calorimetry

  • 1. Ms. Neha S. Raut M.Pharm DIFFERENTIAL THERMAL ANALYSIS & DIFFERENTIAL SCANNING CALORIMETRY Smt. Kishoritai Bhoyar College of Pharmacy, Kamptee
  • 2. INTRODUCTION Differential thermal analysis is a technique measuring the difference in temperature between a sample and reference (a thermally inert material) as a function of the time or the temperature, when they undergo temperature scanning in a controlled atmosphere. The DTA method enables any transformation to be detected for all the categories of materials.
  • 3. Here, Differential temperature ∆T (Temperature difference between sample temperature Ts & reference temperature Tr.) ∆T = Ts – Tr Reference temperature Tr or furnace temperature Tf & ∆T is plotted as a function of time. DTA curve
  • 4. From the graph, ▪ Sharp exothermic peaks give the ideas of changes in crystallity or fusion process. ▪ Chemical reaction (Oxidative reaction) shows Exothermic curve. ▪ Broad endothermic peaks gives signifying dehydration reaction. ▪ Physical changes shows Endothermic curve. ▪ DTA curve would be parallel to the temperature (or time) axis till the sample undergo any physical or chemical changes.
  • 5. INSTRUMENTATION Component of a DTA apparatus  Furnace  Sample Holder  DC Amplifier  Differential Temperature Detector  Furnace Temperature Programmer  Recorder  Control Equipment
  • 6. Diagram of DTA apparatus
  • 7. SAMPLE HOLDER 1.Material Criteria for selection of material ▪ Cost ▪ Ease of fabrication ▪ Inertness towards the reactants & product in the temperature range. Types of material ➢ Metallic material: High thermal conductivity Ex. Nickel, Stainless steel (up to 1000oC), Platinum and its alloys. Give sharp exotherm and flat endotherm.
  • 8. ➢ Non metallic material: Low thermal conductivity Ex. Glass,Vitrous silica or sintered alumina. Give flat exotherm and sharp endotherm. Generally platinum is used. Disadvantage: Catalyses many reactions. 2. Geometry Ideal geometry around thermocouple junction is spherical but show problem in fabricaion.Hence cylindrical shape generally used.
  • 9.  Types of sample holders Sample holder with dimples in which thermocouple junctions are inserted,dimples known as thermocouple well. To investigate several samples simultaneously blocks with symmetrically located multiple compartments have been designed.
  • 10. The reference temperature may be measured either at the center of reference or sample using respective arm of the differential thermocouple in (A) By a separate thermocouple in block (B) (A) (B)
  • 11.  Polyp late sample holder and wire gauge crucibles are used for a good exchange of gases with the enveloping environment, where the solid gas reactions are influenced by the partial pressure of the gaseous reactant or product.
  • 12. FURNACE The choice of furnace geometry and heating element mainly depend upon the length of uniform temperature zone desired. The furnace which cover the range from -1900C to 28000C Heated by A resistance element: nichrome, platinum ,rhodium globar, molybdenum and tungsten. IR Radiation High frequency RF oscillator By a coil of tubing through which a heated or cooled liquid or gas is circulated. Always prefer tubular furnace.
  • 13.  A relation between the power demand P in watts, furnace dimension and temperature for a cylindrical tubular furnace. P = 2.729Km (T1 – T2) l log d2 / d1 Where, l = length in cm Km= Average thermal conductivity coefficient of the insulation(Watt/cm2. K) d1=Diameter of the heater coil wound on the ceramic d2=Diameter of furnace shell T1&T2=Temperature of heating element and surface temperature of the furnace shell
  • 14. TEMPERATURE CONTROLLER & RECORDER Temperature control To control temperature, three basic elements are required. ➢ Sensor ➢ Control element ➢ Heater Control element governs the rate of heat input match with heat loss from the system.
  • 15. Two methods for controlling temperature: On-Off control: In this device, if the sensor signal indicates that the temperature increases than the set point, then the heater immediately cut off. Not use in DTA(Reason-Electrical interference affect measurement of signals). Proportional control: The heat input to the system is progressively reduced as the temperature approaches to the desired value. such controller that anticipates to set value is known as “proportional controller”
  • 16. Temperature Programmer To produce desired rate of heating, cooling and to maintain the constant temperature at any desired value, thermal apparatus require time dependent temperature cycling of the furnace. To achieve this, a temperature programmer which transmits a certain time based instruction to control unit. Recorder The signals obtained from the sensor recorded. Signal trace is produce on paper or film ,heating stylus, electrical writing or optical beam. ▪ Deflection type ▪ Null type
  • 17. I) Deflection Balances:- a) Beam type:- In this type of balance, the conversion of beam deflection about the fulcrum into suitably identified weight change curve by photographic recorded trace. b) Helical or spring balance:- In this type, the elongation or contraction of spring with weight change can be determined.
  • 18. c)Cantilever type:- In this one of the beam is fixed & other end on which sample is to be placed is free to undergo deflection. d)Torsion type:- Beam is attached to the taut wire which act as fulcrum. The wire is finally fixed at both the end so that the deflection of beam are proportional to weight change & tortional strain of wire.
  • 19. II)Null Point Balance:- ▪ In this type there is sensor to detect deviation of the balance beam from the null position. ▪ The restoring force either electrical or mechanical weight loading is applied to restore its null position from the horizontal norm. ▪ The force is directly proportional to weight change.
  • 20. THERMOCOUPLE (TEMPERATURE SENSOR) Selection criteria :  Temperature interval  Thermoelectric coefficient  Chemical capability with sample  Chemical gaseous environment used and reproducibility of EMF Vs. Temperature curve as a function of thermal cycling.  Availability and cost
  • 21. THERMOCOUPLE TEMPERATURE Copper couple Up to 3000C Cromel - alumel couple Up to 10000C Platinum couple Up to 15000C Tungsten & Rhenium in inert gas or vacuum Up to 21000C (not for general use)
  • 22. FACTORS AFFECTING ON DTA CURVE: Environmental :- The DTA technique is more sensitive to gases around sample than TG. Reaction of gases with sample may give extra peaks in curve (i.e. oxygen in air gives oxidation reaction producing exothermic peaks). So to control such reaction DTA studies used two type of gaseous atmosphere. ▪Static ▪Dynamic ▪ Static:-it is difficult to reproduce because atmosphere surrounding the sample changing in the concentration chemically due to evolved gases and physically due to convention current therefore the studies in the static gaseous environment is imprecise. ▪ Dynamic:- Easy to reproduced. gases are swept pass the sample at controlled way are reliable and reproducible. This swept gases are either inert or reactive.
  • 23. Instrumental:- a)Sample holder:- Geometry & the material used in the fabrication of the sample affects the resolution , shape, size of the DTA peaks. ❑ If sample holder made up of , 1. High thermal conductivity material (metal)- sharp exothermic but relatively flat endothermic peak . 2. Poor thermal conductivity material (ceramic)-the reveres will happen. For better resolution the size of the holder and amount of sample should be as small as possible. b)Differential temperature sensing devices:- Generally wires are used. 1. If thick wire is used:- more distortion of peak height & peak temperature. 2. If thinner:- lesser distortion in peak height and peak temperature.
  • 24. c) Furnace characteristics:- 1. Type of winding directly affects the DTA curve. If the winding used in furnace is not uniform, the base line is changed. This type of effect is generally seen in hand wound furnaces. i) Grooved muffled cores furnace is used because it insure uniform winding. ii) Biflar winding also used because it minimize the magnetic pick-up encountered with on –off controller. d) Temperature programmer controller:- Switching on –off type controller are not used because it produces noise at a particular temperature range i.e. a. bow 700oc. Motor driver is used.
  • 25. e) Thermal Regime:- ➢ Heating rate influence the DTA curve. ➢ Higher the heating rates ,higher the peak temperature& sharper the peak intensity. Generally heating rate of 100 to 200 per minute are employed. f) Recorder:- ➢ Type, span, chart-speed and pen response ,sensitivity of recorder affect the DTA curve. ➢ Span is not proper then necessary to preamplify the signals. ➢ If sensitivity is not properly selected, weaker signals would not be recorded whereas stronger signals might be damping. ➢ If faster chart-speeds used , DTA curve gets flattened.
  • 26.  Sample characteristics:- a) physical:- ▪ one assumption that heat capacity remain constant with the progress of reaction but it changes with progress of reaction. ▪ To maintain the heat capacity nearly constant , the usual sample is mixed with an excess amount of an inert material. But it create some problems. ▪ Partial size affects the peak area , it deceases with increasing particle size. ▪ Partial size affects the peak temperature. Increase particle size the peak temperature is shifted to higher value.
  • 27. ▪ Weight of sample also affect the peak intensity & temperature. Both this increases with increasing weight. ▪ To minimize all this problems sample is mixed with a diluents. b) Chemical :- ➢ The chemical reactivity of sample, sample holder, thermocouple material, the ambient gaseous environment and added diluents alters the DTA curve(peaks) . ➢ Select this material inert chemically as possible.
  • 28. APPLICATION 1. Physical chemistry a. Heat of Reaction: Borchardt & Daniels concluded that the peak area A in DTA is always a linear function of the heat of reaction, ∆H, when the rate of heat of production or consumption is a function only of time. The heat of reaction per mole is given by ∆H =KA/N0 Where, N0 = Initial no. of moles K= Constant (Calibration coefficient)
  • 29. b. Specific heat DTA used to determine the specific heat of substance like naphthalene. The Cp was determined by following formula: KK| (b – a) Cp = d ms dt where, K & K| = Constant (determined from calibration curve of standard substance) d = Density of sample ms = Mass of sample dt = The temperature interval over which Cp is measured.
  • 30. c. Thermal diffusivity To determine thermal diffusivities by measuring the temperature difference ,∆T, between the center and surface of the sample, heated at uniform rate. The difference in temperature was measured by using differential thermocouple. ß r2 D = 6 ∆Ts where, r = Radius of spherical sample cavity ß = Heating state
  • 31. 2. Analytical Chemistry a. Polymer analysis Analysis of a polymer shows several features due to physical and chemical changes, including:  Glass transition: Transition from disordered solid to liquid, glassy, amorphous polymer becomes flexible, H = 0, but change in Cp.  Crystallization of amorphous polymer into microcrystal is exothermic. Disordered to ordered transition.  Melting of polymer crystal. Ordered to disordered transition Oxidation peak would be absent in N2 atmosphere
  • 32.  T b. To fingerprint substances DTA of (a) butter and (b) margarine temp → a b c. To determine M.Pt., B.Pt., decomposition temperatures of organic compounds DTA of benzoic acid A ambient pressure; B 200 lb in-2 pressure
  • 33. 3. Quality control DTA technique used for quality control of substance like cement, glass, oil, catalysts, textile, explosives, resins , etc.  Characterization of limestone used in Portland cement  To control amount of magnesium carbonate in cement  To establish slag content present in a mixture of Portland cement & blast furnace slag  Characterization of gypsum plasters & corcidolite.
  • 34. 4.INORGANIC CHEMISTRY  To study the thermal stability of large number of inorganic compound and complexes.  To study oxalates, metal amine complexes, carbonates and oxides.  To study the oxides of uranium and plutonium. Uranium dioxide powder with good sintering qualities has been observed to give well defined and well separated DTA peaks.
  • 35.  Advantages: • instruments can be used at very high temperatures • instruments are highly sensitive • flexibility in crucible volume/form • characteristic transition or reaction temperatures can be accurately determined  Disadvantages: • uncertainty of heats of fusion, transition, or reaction estimations is 20-50% • less satisfactory than DSC with regard to resolution of thermal traces and qualitative data.
  • 36. INTRODUCTION Differential scanning calorimetric is a technique determining the variation in the heat flow given out or taken in by a sample as a function of temperature or time. The DSC curve is recorded with the chart abscissa indicating the transition temperature . The area of peak measures the total energy transfer to or from the sample.
  • 37. INSTRUMENTATION ➢ A typical DSC consists of two sealed pans: a sample pan and a reference pan(empty). These pans are often covered by or composed of aluminum, which acts as a radiation shield. The two pans are heated, or cooled, uniformly while the heat flow difference between the two is monitored. ➢ This can be done at a constant temperature (isothermally), but is more commonly done by changing the temperature at a constant rate, a mode of operation also called temperature scanning. ➢ The instrument detects differences in the heat flow between the sample and reference.
  • 38. ➢ This information is sent to an output device, most often a computer, resulting in a plot of the differential heat flow between the reference and sample cell as a function of temperature. the differential heat flow is calculated by subtracting the sample heat flow from the reference heat flow. ➢ The sample is generally placed in an aluminum sample pan. The reference consists of a matched empty aluminum sample pan that is placed in the reference cell of the instrument. The sample pans are designed to have a very high thermal conductivity. ➢ Sample sizes generally range from 0.1 to 100 mg. This also allows experiments to be performed under variable pressures and atmospheres.
  • 39. TYPES OF DSC INSTRUMENT 1.Heat Flux DSC:- sample pan inert gas vacuum heating coil reference pan thermocouples chromel wafer constantan chromel/calomel wires crimped Al pans (<500 o C)
  • 40. ▪ sample holder : sample and reference are connected by a low-resistance heat flow path Al or Pt pans placed on constantan disc ▪ Sensors: Chromel®-constantan area thermocouples (differential heat flow) Chromel®-alumel thermocouples (sample temperature) ▪ Furnace: One block for both sample and reference cells ▪ temperature controller: temperature difference between the sample and reference is converted to differential thermal power, did/dot, which is supplied to the heaters to maintain the temperature of the sample and reference at the program value
  • 41. 2.Power Compensated DSC sample pan T = 0 inert gas vacuum inert gas vacuum individual heaters controller P reference pan thermocouple
  • 42.  Sample holder: Al or Pt pans  Sensors: Pt resistance thermocouples separate sensors and heaters for the sample and reference  Furnace: separate blocks for sample and reference cells  Temperature controller: differential thermal power is supplied to the heaters to maintain the temperature of the sample and reference at the program value
  • 43. FACTORS AFFECTING DSC CURVES a. Sample shape: The shape of sample has little effect on quantitative aspect but more effect on quality aspect. Sample in the form of a disc film or powder spread on the pan are preferred.
  • 44. b. Sample size 0.5 to 10mg usually sufficient. Smaller sample: ▪ Faster scanning ▪ Better shaped peak with good resolution ▪ Provide greater contact with the gaseous environment Larger sample  Smaller heat of transitions may be measured with greater precision. c. Power supply ; Variation of power supply to sample & reference DSC curve
  • 45. APPLICATION DSC can be used for all application of conventional DTA. Use in industry for small size of sample To detect phase changes and decompositions. Ex.- DTA & DSC of CuSO4 .5H2O DTA DSC
  • 46. To study the oxidative stability of samples generally requires an airtight sample chamber. Usually, such tests are done isothermally (at constant temperature) by changing the atmosphere of the sample. First, the sample is brought to the desired test temperature under an inert atmosphere, usually nitrogen. Then, oxygen is added to the system. Any oxidation that occurs is observed as a deviation in the baseline. Such analyses can be used to determine the stability and optimum storage conditions for a compound. Consequently, less pure compounds will exhibit a broadened melting peak that begin sat lower temperature than a pure compound.
  • 47. In the pharmaceutical industry it is necessary to have well-characterized drug compounds in order to define processing parameters. For instance, if it is necessary to deliver a drug in the amorphous form, it is desirable to process the drug at temperatures below those at which crystallization can occur. In food science research, DSC is used in conjunction with other thermal analytical techniques to determine water dynamics. Changes in water distribution may be correlated with changes in texture. Similar to material science studies, the effects of curing on confectionery products can also be analyzed.
  • 48. In last few years this technology has been involved in metallic material study. It is known that it is possible to use DSC to find solids and liquids temperature of a metal alloy, but the widest application is, by now, the study of precipitations, Gainer Preston zones, phase transitions, dislocations movement, grain growth etc. For the polymer chemist, DSC is a handy tool for studying curing processes, which allows the fine tuning of polymer properties. The cross-linking of polymer molecules that occurs in the curing process is exothermic, resulting in a positive peak in the DSC curve that usually appears soon after the glass transition.
  • 49. DSC curves may also be used to evaluate drug and polymer purities. This is possible because the temperature range over which a mixture of compounds melts is dependent on their relative amounts. This effect is due to a phenomenon known as freezing point depression, which occurs when a foreign solute is added to a solution. Used in the study of liquid crystals. As matter transitions between solid and liquid it often goes through a third state, which displays properties of both phases. This anisotropic liquid is known as a liquid crystalline or mesomorphous state. Using DSC, it is possible to observe the small energy changes that occur as matter transitions from a solid to a liquid crystal and from a liquid crystal to an isotropic liquid.
  • 50.  Advantages • Smaller sample required. • Good qualitative data on phase changes.  Disadvantages • Limited to small sample size • Thermograms are often complex and thus difficult to interpret fully
  • 51. COMPARISON OF DTA AND DSC Aspect DSC DTA Size of sample 2 to 10mg 20 to 50 mg Sensitivity of measurement of heat of transition A few joules/mole 0.5 Kj/mole Heating and cooling cycle Programmed heating and cooling possible Generally programmed heating. Second order phase transition It can be observed with a sample size of 200mg Not observed. Specific heat measurement Accurate Not accurate