• Stress corrosion cracking is a failure mechanism that is
caused by environment, susceptible material, and tensile
stress. Temperature is a significant environmental factor
affecting cracking.
“OR”
A structure under static tensile stress, much below the
yield stress, in contact with corrosive environment may fail
due to SCC. Three conditions must be present
simultaneously to produce SCC: a critical corrosive
environment, a susceptible alloy and some component of
tensile stress.
Now the phenomena of “SCC” is shown in the
following figures
Cont’d
• SCC leads to the formation of a crack which would not
have developed by the action of the stress or environment
alone. It is the unexpected sudden failure of normally
ductile metals subjected to a tensile stress in a corrosive
environment.
• The required tensile stresses may be in the form of
directly applied stresses or in the form of residual stresses.
Causes of SCC
• There are three main causes for SCC as given follows:
• Corrosive Environments
• Tensile Stresses Above Threshold
• A Susceptible Material
Cont’d
• Common sources of tensile stresses are:
1: External stresses caused by
•Centrifugal forces
•Temperature variation
2: Residual stresses due to
•Forming
•Heat treatment
•Welding
•Machining
•Grinding
Cont’d
3: Concentration of stresses at the root of pre-existing cracks or
notches
Stages Involved In SCC
• The process of SCC consists of three stages:
• Crack Initiation
• Crack Propagation
• Brittle Fracture
Crack Initiation
• SCC is initiated by stress concentrations at
defects on the material surface. The defect may
be an existing material defect. The defect may
also be a result of pitting corrosion, crevice
corrosion, intergranular corrosion or local
galvanic corrosion.
Crack Propagation
• The passivation film at the tip of the crack is broken
due to plastic deformation. Pure and normally very
active metal is exposed and will be attacked by
corrosion. Grow rate will be a combination of corrosion
and cracking. The crack starts to grow when the stress
concentration at the end of the crack (KI) exceeds the
threshold stress intensity factor for stress corrosion
cracking (KISCC).
Brittle Fracture
• When the stress concentration at the end of the
crack exceeds the critical stress intensity factor
(KI > KIC), there will be a rapid, unstable brittle
fracture.
Examples
• Many materials, particularly high strength materials, are
susceptible to stress corrosion cracking when exposed to a
specific environment. For example, cold worked brass,
which is found in ammunition cartridges, is susceptible to
stress corrosion cracking when exposed to an environment
containing ammonia. In chloride containing environments,
titanium alloys, aluminum alloys, and high
strength stainless steels are susceptible and specific alloys,
which are resistant to stress corrosion cracking, should be
used. The stresses required to initiate and propagate
cracking are often low and many failures occur due to
residual stresses rather than applied stress.
Ways Of Propagation Of SCC
• SCC can proceed in either of two ways :
• Intergranular Stress Corrosion Cracking
• Transgranular Stress Corrosion Cracking
Intergranular SCC
• The cracks which propagate along the grain boundaries
called as intergranular stress corrosion cracking as
shown in the following figures.
Transgranular SCC
• The cracks which run through the individual grains
called as transgranular stress corrosion cracking as
shown in the following figures.
Identification Of
SCC
• Visual identification prior to failure is difficult
due to the typical tightness of stress-corrosion
cracks. A low-power hand lens will greatly aid
determination. Detection of cracks can also be
enhanced with ultrasonic, radiographic, or
acoustic emission techniques.
Preventive Measures
• There are a number of different ways to control SCC. The method
used depends on the application and may involve changing the
mechanical, metallurgical and environmental conditions.
• Mechanical
• Avoid stress concentrators
• Relieve fabrication stresses
• Introduce surface compressive stresses
• Reduce operating stresses
• Metallurgical
• Change alloy composition
• Change alloy structure
• Use metallic conversion coating
• Environmental
• Add inhibitor
• Modify temperature
Stress corrosion cracking

Weitere ähnliche Inhalte

Was ist angesagt?

Hydrogen embrittlement of steels
Hydrogen embrittlement of steelsHydrogen embrittlement of steels
Hydrogen embrittlement of steelsvishnu90
 
Hydrogen Embrittlement : Causes, Effects, Prevention.
Hydrogen Embrittlement : Causes, Effects, Prevention.Hydrogen Embrittlement : Causes, Effects, Prevention.
Hydrogen Embrittlement : Causes, Effects, Prevention.Sidheshwar Kumar
 
HOT CRACKS AND COLD CRACKS (Welding)
HOT CRACKS AND COLD CRACKS (Welding)HOT CRACKS AND COLD CRACKS (Welding)
HOT CRACKS AND COLD CRACKS (Welding)Melwin Dmello
 
Corrosion Monitoring
Corrosion MonitoringCorrosion Monitoring
Corrosion MonitoringDhanesh S
 
Thermal spray coating
Thermal spray coatingThermal spray coating
Thermal spray coatingJMB
 
Surface coatings, hardfacing,thermal spraying
Surface coatings, hardfacing,thermal sprayingSurface coatings, hardfacing,thermal spraying
Surface coatings, hardfacing,thermal sprayinggidla vinay
 
Ductile to brittle transition
Ductile to brittle transitionDuctile to brittle transition
Ductile to brittle transitionBilal
 
Corrosion engineering
Corrosion engineeringCorrosion engineering
Corrosion engineeringArif Raihan
 
creep deformation of the Materials
 creep deformation of the   Materials creep deformation of the   Materials
creep deformation of the Materialsengomar84
 
selective leaching type corrosion
selective leaching type corrosionselective leaching type corrosion
selective leaching type corrosionJAYESH PAREKH
 
Tests for intergranular corrosion and stress corrosion cracking
Tests for intergranular corrosion and stress corrosion crackingTests for intergranular corrosion and stress corrosion cracking
Tests for intergranular corrosion and stress corrosion crackingkoshykanjirapallikaran
 

Was ist angesagt? (20)

Hydrogen embrittlement of steels
Hydrogen embrittlement of steelsHydrogen embrittlement of steels
Hydrogen embrittlement of steels
 
Wear ppt
Wear pptWear ppt
Wear ppt
 
Hydrogen Embrittlement : Causes, Effects, Prevention.
Hydrogen Embrittlement : Causes, Effects, Prevention.Hydrogen Embrittlement : Causes, Effects, Prevention.
Hydrogen Embrittlement : Causes, Effects, Prevention.
 
HOT CRACKS AND COLD CRACKS (Welding)
HOT CRACKS AND COLD CRACKS (Welding)HOT CRACKS AND COLD CRACKS (Welding)
HOT CRACKS AND COLD CRACKS (Welding)
 
Corrosion Monitoring
Corrosion MonitoringCorrosion Monitoring
Corrosion Monitoring
 
Thermal spray coating
Thermal spray coatingThermal spray coating
Thermal spray coating
 
FRACTURE BEHAVIOUR
FRACTURE BEHAVIOURFRACTURE BEHAVIOUR
FRACTURE BEHAVIOUR
 
Surface coatings, hardfacing,thermal spraying
Surface coatings, hardfacing,thermal sprayingSurface coatings, hardfacing,thermal spraying
Surface coatings, hardfacing,thermal spraying
 
Ductile to brittle transition
Ductile to brittle transitionDuctile to brittle transition
Ductile to brittle transition
 
Corrosion
CorrosionCorrosion
Corrosion
 
Fracture Mechanics & Failure Analysis:Lectures Fractrography
Fracture Mechanics & Failure Analysis:Lectures Fractrography  Fracture Mechanics & Failure Analysis:Lectures Fractrography
Fracture Mechanics & Failure Analysis:Lectures Fractrography
 
Wear of Metals
Wear of MetalsWear of Metals
Wear of Metals
 
Stress Corrosion Cracking.pptx
Stress Corrosion Cracking.pptxStress Corrosion Cracking.pptx
Stress Corrosion Cracking.pptx
 
Corrosion engineering
Corrosion engineeringCorrosion engineering
Corrosion engineering
 
Fatigue and creep
Fatigue and creepFatigue and creep
Fatigue and creep
 
creep deformation of the Materials
 creep deformation of the   Materials creep deformation of the   Materials
creep deformation of the Materials
 
selective leaching type corrosion
selective leaching type corrosionselective leaching type corrosion
selective leaching type corrosion
 
Forms Of Corrosion
Forms Of CorrosionForms Of Corrosion
Forms Of Corrosion
 
Fracture Mechanics & Failure Analysis: creep and stress rupture
Fracture Mechanics & Failure Analysis: creep and stress ruptureFracture Mechanics & Failure Analysis: creep and stress rupture
Fracture Mechanics & Failure Analysis: creep and stress rupture
 
Tests for intergranular corrosion and stress corrosion cracking
Tests for intergranular corrosion and stress corrosion crackingTests for intergranular corrosion and stress corrosion cracking
Tests for intergranular corrosion and stress corrosion cracking
 

Andere mochten auch (13)

Corrocion bajo tension mrgm civil
Corrocion bajo tension mrgm civilCorrocion bajo tension mrgm civil
Corrocion bajo tension mrgm civil
 
Tipos de corrosión
Tipos de corrosiónTipos de corrosión
Tipos de corrosión
 
Como evitar la corrrosion
Como evitar la corrrosion Como evitar la corrrosion
Como evitar la corrrosion
 
Corrosión por picaduras
Corrosión por picadurasCorrosión por picaduras
Corrosión por picaduras
 
corrosion en la industria petroquimica
corrosion en la industria petroquimicacorrosion en la industria petroquimica
corrosion en la industria petroquimica
 
Presentación corrosión
Presentación corrosiónPresentación corrosión
Presentación corrosión
 
SCC Research Guide
SCC Research GuideSCC Research Guide
SCC Research Guide
 
Corrosion
CorrosionCorrosion
Corrosion
 
TIPOS DE CORROSIÓN
TIPOS DE CORROSIÓNTIPOS DE CORROSIÓN
TIPOS DE CORROSIÓN
 
Corrosion
CorrosionCorrosion
Corrosion
 
3 mecanismos corrosion
3 mecanismos corrosion3 mecanismos corrosion
3 mecanismos corrosion
 
Corrosion
CorrosionCorrosion
Corrosion
 
Corrosión en metales parte 2
Corrosión en metales parte 2 Corrosión en metales parte 2
Corrosión en metales parte 2
 

Ähnlich wie Stress corrosion cracking

Stress corrosion cracking
Stress corrosion crackingStress corrosion cracking
Stress corrosion crackingpranav52906
 
Chapter 12_SCC.pdf
Chapter 12_SCC.pdfChapter 12_SCC.pdf
Chapter 12_SCC.pdfssuserca7f42
 
Corrosion in implants by Haleeful jud
Corrosion in implants by Haleeful judCorrosion in implants by Haleeful jud
Corrosion in implants by Haleeful judhaleeful jud
 
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptxSahalSachu
 
Case Study on Failure Due to Fatigue
Case Study on Failure Due to FatigueCase Study on Failure Due to Fatigue
Case Study on Failure Due to FatigueAbhijit Debnath
 
Environmentally assisted failures in metallic and composite materials
Environmentally assisted failures in metallic and composite materials Environmentally assisted failures in metallic and composite materials
Environmentally assisted failures in metallic and composite materials Padmanabhan Krishnan
 
CH-2,3&4 Maintenance (1).pptx
CH-2,3&4 Maintenance (1).pptxCH-2,3&4 Maintenance (1).pptx
CH-2,3&4 Maintenance (1).pptxBarsena
 
Presentation on corrosion
Presentation on corrosionPresentation on corrosion
Presentation on corrosionshubham singh
 
Lec3 failure.pptx introductionto fialure types and causes
Lec3 failure.pptx introductionto fialure types and causesLec3 failure.pptx introductionto fialure types and causes
Lec3 failure.pptx introductionto fialure types and causesssuserac3f5b
 
Metal corrosion and its prevention
Metal corrosion and its preventionMetal corrosion and its prevention
Metal corrosion and its preventionDr. Sandip Thorat
 
Corrosion metallurgy
Corrosion metallurgyCorrosion metallurgy
Corrosion metallurgyAhmed Awad
 
Corrosion control in_engineering_design
Corrosion control in_engineering_designCorrosion control in_engineering_design
Corrosion control in_engineering_designAli Zamel
 
Corrosion of Spring 2013 ASM Presentation
Corrosion of Spring 2013 ASM PresentationCorrosion of Spring 2013 ASM Presentation
Corrosion of Spring 2013 ASM PresentationRobert OShea, Jr., P.E.
 
Mme 323 materials science week 11-12 - failure
Mme 323 materials science   week 11-12 - failureMme 323 materials science   week 11-12 - failure
Mme 323 materials science week 11-12 - failureAdhi Primartomo
 
Fracture mechanics
Fracture mechanicsFracture mechanics
Fracture mechanicsmanojg1990
 
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2Kunduru Srinivasulu Reddy
 

Ähnlich wie Stress corrosion cracking (20)

Stress corrosion cracking
Stress corrosion crackingStress corrosion cracking
Stress corrosion cracking
 
Chapter 12_SCC.pdf
Chapter 12_SCC.pdfChapter 12_SCC.pdf
Chapter 12_SCC.pdf
 
Corrosion in implants by Haleeful jud
Corrosion in implants by Haleeful judCorrosion in implants by Haleeful jud
Corrosion in implants by Haleeful jud
 
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx
1655475850538_METALLURGY AND MATERIAL SCIENCE.pptx
 
corrosion presentation
corrosion presentationcorrosion presentation
corrosion presentation
 
Case Study on Failure Due to Fatigue
Case Study on Failure Due to FatigueCase Study on Failure Due to Fatigue
Case Study on Failure Due to Fatigue
 
Environmentally assisted failures in metallic and composite materials
Environmentally assisted failures in metallic and composite materials Environmentally assisted failures in metallic and composite materials
Environmentally assisted failures in metallic and composite materials
 
CH-2,3&4 Maintenance (1).pptx
CH-2,3&4 Maintenance (1).pptxCH-2,3&4 Maintenance (1).pptx
CH-2,3&4 Maintenance (1).pptx
 
Failure Analysis.pptx
Failure Analysis.pptxFailure Analysis.pptx
Failure Analysis.pptx
 
Presentation on corrosion
Presentation on corrosionPresentation on corrosion
Presentation on corrosion
 
Lec3 failure.pptx introductionto fialure types and causes
Lec3 failure.pptx introductionto fialure types and causesLec3 failure.pptx introductionto fialure types and causes
Lec3 failure.pptx introductionto fialure types and causes
 
Metal corrosion and its prevention
Metal corrosion and its preventionMetal corrosion and its prevention
Metal corrosion and its prevention
 
Corrosion metallurgy
Corrosion metallurgyCorrosion metallurgy
Corrosion metallurgy
 
Corrosion control in_engineering_design
Corrosion control in_engineering_designCorrosion control in_engineering_design
Corrosion control in_engineering_design
 
Corrosion of Spring 2013 ASM Presentation
Corrosion of Spring 2013 ASM PresentationCorrosion of Spring 2013 ASM Presentation
Corrosion of Spring 2013 ASM Presentation
 
Seminar on fatigue
Seminar on fatigueSeminar on fatigue
Seminar on fatigue
 
Mme 323 materials science week 11-12 - failure
Mme 323 materials science   week 11-12 - failureMme 323 materials science   week 11-12 - failure
Mme 323 materials science week 11-12 - failure
 
Fracture mechanics
Fracture mechanicsFracture mechanics
Fracture mechanics
 
Corrosion
CorrosionCorrosion
Corrosion
 
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2
K.Srinivasulureddy-SNIST-Metallurgy & Material Science-UNIT-2
 

Mehr von onlinemetallurgy.com (20)

WATER JET CUTTING
WATER JET CUTTINGWATER JET CUTTING
WATER JET CUTTING
 
Twinning
TwinningTwinning
Twinning
 
TTT diagram of eutectoid steel and martensitic transformation
TTT diagram of eutectoid steel and martensitic transformationTTT diagram of eutectoid steel and martensitic transformation
TTT diagram of eutectoid steel and martensitic transformation
 
Tolerances and allowances
Tolerances and allowancesTolerances and allowances
Tolerances and allowances
 
Tolerance and allowance 2
Tolerance and allowance 2Tolerance and allowance 2
Tolerance and allowance 2
 
Time temperature transformation curves 2
Time temperature transformation curves 2Time temperature transformation curves 2
Time temperature transformation curves 2
 
Thorium
ThoriumThorium
Thorium
 
The structure and properties of polymers
The structure and properties of polymersThe structure and properties of polymers
The structure and properties of polymers
 
Stainless steel in nuclear
Stainless steel in nuclearStainless steel in nuclear
Stainless steel in nuclear
 
Shore hardness
Shore hardnessShore hardness
Shore hardness
 
Sheet forming
Sheet formingSheet forming
Sheet forming
 
Rusting of fe and ss
Rusting of fe and ssRusting of fe and ss
Rusting of fe and ss
 
Rolling
RollingRolling
Rolling
 
Radioactivity & waste
Radioactivity & wasteRadioactivity & waste
Radioactivity & waste
 
Radiation hazards
Radiation hazardsRadiation hazards
Radiation hazards
 
Ultrasonic hardness testing
Ultrasonic hardness testingUltrasonic hardness testing
Ultrasonic hardness testing
 
Gas cooled reactors
Gas cooled reactorsGas cooled reactors
Gas cooled reactors
 
Fiber manufacturing
Fiber manufacturingFiber manufacturing
Fiber manufacturing
 
Hardness testing
Hardness testingHardness testing
Hardness testing
 
Precipitation hardening
Precipitation hardeningPrecipitation hardening
Precipitation hardening
 

Stress corrosion cracking

  • 1.
  • 2. For more help contact me Muhammad Umair Bukhari Engr.umair.bukhari@gmail.com http://onlinemetallurgy.com
  • 3. • Stress corrosion cracking is a failure mechanism that is caused by environment, susceptible material, and tensile stress. Temperature is a significant environmental factor affecting cracking. “OR” A structure under static tensile stress, much below the yield stress, in contact with corrosive environment may fail due to SCC. Three conditions must be present simultaneously to produce SCC: a critical corrosive environment, a susceptible alloy and some component of tensile stress.
  • 4. Now the phenomena of “SCC” is shown in the following figures
  • 5. Cont’d • SCC leads to the formation of a crack which would not have developed by the action of the stress or environment alone. It is the unexpected sudden failure of normally ductile metals subjected to a tensile stress in a corrosive environment. • The required tensile stresses may be in the form of directly applied stresses or in the form of residual stresses.
  • 6.
  • 7. Causes of SCC • There are three main causes for SCC as given follows: • Corrosive Environments • Tensile Stresses Above Threshold • A Susceptible Material
  • 8.
  • 9. Cont’d • Common sources of tensile stresses are: 1: External stresses caused by •Centrifugal forces •Temperature variation 2: Residual stresses due to •Forming •Heat treatment •Welding •Machining •Grinding
  • 10. Cont’d 3: Concentration of stresses at the root of pre-existing cracks or notches
  • 11. Stages Involved In SCC • The process of SCC consists of three stages: • Crack Initiation • Crack Propagation • Brittle Fracture
  • 12. Crack Initiation • SCC is initiated by stress concentrations at defects on the material surface. The defect may be an existing material defect. The defect may also be a result of pitting corrosion, crevice corrosion, intergranular corrosion or local galvanic corrosion.
  • 13.
  • 14. Crack Propagation • The passivation film at the tip of the crack is broken due to plastic deformation. Pure and normally very active metal is exposed and will be attacked by corrosion. Grow rate will be a combination of corrosion and cracking. The crack starts to grow when the stress concentration at the end of the crack (KI) exceeds the threshold stress intensity factor for stress corrosion cracking (KISCC).
  • 15. Brittle Fracture • When the stress concentration at the end of the crack exceeds the critical stress intensity factor (KI > KIC), there will be a rapid, unstable brittle fracture.
  • 16. Examples • Many materials, particularly high strength materials, are susceptible to stress corrosion cracking when exposed to a specific environment. For example, cold worked brass, which is found in ammunition cartridges, is susceptible to stress corrosion cracking when exposed to an environment containing ammonia. In chloride containing environments, titanium alloys, aluminum alloys, and high strength stainless steels are susceptible and specific alloys, which are resistant to stress corrosion cracking, should be used. The stresses required to initiate and propagate cracking are often low and many failures occur due to residual stresses rather than applied stress.
  • 17.
  • 18. Ways Of Propagation Of SCC • SCC can proceed in either of two ways : • Intergranular Stress Corrosion Cracking • Transgranular Stress Corrosion Cracking
  • 19. Intergranular SCC • The cracks which propagate along the grain boundaries called as intergranular stress corrosion cracking as shown in the following figures.
  • 20. Transgranular SCC • The cracks which run through the individual grains called as transgranular stress corrosion cracking as shown in the following figures.
  • 21. Identification Of SCC • Visual identification prior to failure is difficult due to the typical tightness of stress-corrosion cracks. A low-power hand lens will greatly aid determination. Detection of cracks can also be enhanced with ultrasonic, radiographic, or acoustic emission techniques.
  • 22. Preventive Measures • There are a number of different ways to control SCC. The method used depends on the application and may involve changing the mechanical, metallurgical and environmental conditions. • Mechanical • Avoid stress concentrators • Relieve fabrication stresses • Introduce surface compressive stresses • Reduce operating stresses • Metallurgical • Change alloy composition • Change alloy structure • Use metallic conversion coating
  • 23. • Environmental • Add inhibitor • Modify temperature