3. ASHOK LEYLAND
Ashok Leyland is the 2nd biggest automobile
manufacturers in India.
Founded in 1948 as ASHOK MOTORS by
Mr.RAGHUNANDAN SARAN, an
Industrialist.
At present there are 6 plants in India, & also
serving in 30 countries around the world.
Mother plant at ENNORE in chennai, in
HOSUR two plants(Unit 1 & Unit 2),ALWAR
in Rajasthan, BHANDARA in Maharashtra &
recently new plant at PANTANAGAR.
4. ASHOK LEYLAND PRODUCES
LCV : Light Commercial Vehicles
MDV : Medium Duty Vehicles
HDV : Heavy Duty Vehicles
ICV : Intermediate Commercial
Vehicles
Recently ASHOK LEYLAND has
stepped in production of Luxury car….
Buses from 18 to 80 seaters are
manufactured.
Trucks ranging from 4.5 tones to 49
tones ……….
5. Second Largest Automobile Vehicle Manufacturer in INDIA
ASHOKLEYLAND and IVECO joint
venture in 1993 – 1994
In 1954, GOVERNMENT approval for
manufacture of commercial vehicles
The name of the company was changed to ASHOK LEYLAND
LIMITED in 1955
Our Defence Vehicle is backbone of INDIAN ARMY
6. Ashok Leyland Passenger Transportation
Ashok Leyland buses carry more than 60 million
passengers everyday, More comparing to Indian
Railways.
Ashok Leyland is the India's only manufacturer of
double‐decker buses.
It head started in alternate energy buses ‐ BS II &
BS III. Eight out of ten metro state transport buses
in India are from Ashok Leyland.
It is one of the leading suppliers of defense vehicles
in the world and also the leading supplier of logistics
vehicles to the Indian Army.
7. What is SKIN PANEL ?
SKIN PANEL is a visual outer
body of a vehicle majorly
CABIN parts……
Proper metal finished
skin panels are very important
for good ASTHETIC LOOK of
a vehicle…….
8. This report Skin Panel
Inspection report is regarding
the ASHOK LEYLAND’s model
named “DOST”.
DOST model is in joint venture
with NISSAN MOTORS.
DOST is awarded as
“LCV of the year 2012”.
10. Continues…..
Basically DOST model has 14 SKIN
PANELS.
Each panel is identified by a Part
No.
All panels are stamped(pressed) in
ASHOK LEYLAND press shop.
Sheet metal thickness ranges from
0.7mm to 1.6mm.
11. The 14 skin panels of DOST are
1) Door outer RH
2) Door outer LH
3) Door inner RH
4) Door inner LH
5) Roof
6) Floor
7) Front Panel
8) Sill outer RH
9) Sill outer LH
10) Corner Panel RH
11) Corner Panel LH
12) Back Panel
13) B Pillar RH
14) B Pillar LH
14. Inspection of Skin Panels
1. Visual inspection is popular way of inspecting skin panels.
2. Manually inspecting by wearing inspection Gloves
3. CMM is used in some critical areas
4. Oil stoning the panel with Oil stone.
Major Defects On Skin Panel
1. DENTS : Dent refers to shallow deformation on the surface of a panel
or object.
Reason :
1. Due to some dust & foreign particles on die surface.
2. Rarely during loading and unloading of panel.
2. PEAKS : Peak refers to a high point on the surface of a panel or object.
Reason :
1. Dust & foreign particles on die surface.
2. During loading & unloading of panel.
16. 3.WRINKLE :
• Wrinkle refers to waviness formed on surface of panel.
• Wrinkle can also be known as high and low areas.
Reason :
1. Low cushion pressure.
2. Varying Cylinder forces.
4.WELDING DAMAGE :
Welding damage means spot damage.
which may damage the channel, flange.
Reason :
1. Due to mislocation.
2. Urgency.
3. Due to Child part defect.
4. Weld burning, blackening.
5. Due to high current value.
5. CRACKS :Crack is a thin & narrow opening in a flat,
solid material.
Before crack THINNING occurs.
Reason :
1. Due to more holding, blanking pressure.
2. Slug mark.
17. Tools used for inspection
1. The most important tool for inspection is OIL
STONE.
2. Hand Gloves.
3. Taper Scale.
4. Pin point micrometer.
5. Vernier Caliper.
6. CMM(Coordinate Measuring Machine).
7. Flash light.
18. METAL FINISHING:-Metal finishing(Rework) is a process which
includes rework of SKIN PANEL DEFECTS, cleaning of panels, providing
proper finish & preparing the panel for next painting stage.
METAL FINISHING OPERATIONS
In this primarily panels will be cleaned from oil, sealant & rust.
Rework of defects will be done in this stage.
For peaks, they will hammer it slowly and will finish with
VERTICAL SANDER then finally with RANDOM ORBITAL
SANDER.
For dents they will use a special equipment called DENT PULLER.
For cracks the solution is welding , grinding & matching the surface.
We use MIG(Metal Inert Gas)welding for cracked surface & also for
thinning.
To remove welded spot in case of weld damage we will use a SPOT
REMOVAEBLE DRILL & after correction it will be welded again.